欢迎访问过程工程学报, 今天是
中国科学院过程工程研究所
Toggle navigation
首页
期刊介绍
期刊简介
主编致辞
所获荣誉
编委会
往届编委会
本届编委会
期刊订阅
投稿指南
出版道德
在线期刊
最新录用
当期目录
过刊浏览
阅读排行
下载排行
引用排行
下载中心
联系我们
English
当期目录
2006年 第6卷 第6期 刊出日期:2006-12-20
上一期
下一期
流动与传递
Numerical Simulation of Macroscopic Mixing in a Rushton Impeller Stirred Tank
王正;毛在砂;沈湘黔
. 2006, 6(6): 857-863.
摘要
(
)
PDF
(236KB) (
)
相关文章
|
计量指标
The macroscopic mixing in a stirred tank with different tracer injection locations, impeller speeds and impeller positions is simulated numerically by solving the transport equation of the tracer based on the whole flow field in the baffled tank with a Rushton disk turbine numerically resolved using the improved inner-outer iterative procedure. Predicted mixing time is compared well with the literature correlations. The predicted residence time distribution of the stirred tank is very close to the present experimental results. The effect of the installation of a draft tube on the mixing time and residence time distributions is addressed.
射流流化床中锥形分布板对流动的影响
洪若瑜
. 2006, 6(6): 864-871.
摘要
(
)
PDF
(749KB) (
)
相关文章
|
计量指标
给出了具有锥形分布板的射流流化床中浓密气固两相流动的多相流体力学基本方程组. 采用二维正交曲线坐标并生成了数值网格,用改进的IPSA方法求解二维正交曲线坐标中的多相流基本方程组,并编制了大型通用程序,流场可视化使用Tecplot软件. 对于给定的模拟计算,计算结果与实验值吻合. 模拟计算中改变了锥形筛板的角度、射流管的直径、床层高度、分布板开孔率的分布、射流气速、床层表观气速等,通过模拟得到床内的流动图像,考察了射流高度及颗粒循环的影响.
操作条件对双循环回路变径提升管压降的影响
王向辉;高士秋;宋文立;许友好;张久顺
. 2006, 6(6): 872-877.
摘要
(
)
PDF
(221KB) (
)
相关文章
|
计量指标
针对生产清洁汽油组分的催化裂化新工艺,建立了具有双循环回路的变径提升管冷模实验装置. 提升管由下部具有较小床径、较高气速的气力输送区和上部具有较大床径、较低气速的快速流化区组成,循环物料可在提升管的下部和中部分别加入,形成主、副两个循环回路. 分析了系统主、副循环回路的压力平衡关系,研究了操作条件对提升管压降的影响. 结果发现,主、副循环回路的提升管压降均随表观气速的增加而降低;增加2个循环回路中任意一个固体循环速率时,将使另一循环回路的固体循环速率降低,但总固体循环速率和2个循环回路的提升管压降均升高. 2个循环回路相互影响并保持各自的压力平衡,在固体循环速率控制阀处,只有循环管端压力大于提升管端压力才能维持系统正常操作. 增加系统藏料量、循环管直径、副循环供料床高度和直径均有利于维持循环系统的正常操作.
液固两相外循环流化床压力波动信号的统计及频谱分析
张少峰;王琦;高川博;刘燕
. 2006, 6(6): 878-883.
摘要
(
)
PDF
(313KB) (
)
相关文章
|
计量指标
压力波动信号是表征流化床内流体运动特性的重要信息. 为了更好地了解液固外循环流化床内流体流动特征,在液固外循环流化床中,对床体壁面压力波动信号进行了时域、频域及自相关性分析. 结果表明,沿床体稳定流化段上的压力波动特征相似,流体流动和颗粒运动所引发的压力波动能量频带分别集中在0~10和30~40 Hz之间,压力波动的概率密度近似呈正态分布,液固两相外循环流化床中的压力波动信号介于周期信号和随机信号之间.
高粘度流体在波纹板通道内的流动模型
师晋生
. 2006, 6(6): 884-888.
摘要
(
)
PDF
(273KB) (
)
相关文章
|
计量指标
对高粘度流体在波纹板通道内的流动进行了分析,对控制微分方程及边界条件作无量纲处理,引入流函数,采用摄动展开建立了近似分析模型,得到了流函数、速度及压力沿轴向变化的解析表达式,讨论了壁面波纹的波幅及波长对流动的影响,并根据比拟理论分析了波纹通道对传热的影响.
流动过冷沸腾传热强化及阻垢
谢云峰;任晓光;宋永吉;王梦璐
. 2006, 6(6): 889-893.
摘要
(
)
PDF
(246KB) (
)
相关文章
|
计量指标
在流动沸腾传热实验中,考察了CaCO3污垢溶液的形成过程及各种工艺条件对流动过冷沸腾传热的影响. 研究条件包括流体速度、溶液温度、CaCO3溶液浓度及热通量,实验中发现了一些规律. 同时还考察了不同阻垢剂[聚天冬氨酸(PASP)、2-膦酸丁烷-1,2,4-三羧酸(PBTCA)及氨基三甲叉膦酸(ATMP)]对流动过冷沸腾传热的影响. 结果表明,所选阻垢剂均能抑制污垢的生成并降低了污垢热阻,而且存在最佳浓度范围. 但不同阻垢剂的阻垢效果不尽相同,在本实验条件下,ATMP的阻垢效果最好,PBTCA次之,PASP的阻垢效果较差.
反应与分离
复杂MeSO4体系初步除杂和深度净化
彭长宏;唐谟堂;黄虹
. 2006, 6(6): 894-898.
摘要
(
)
PDF
(181KB) (
)
相关文章
|
计量指标
分别以浸出液和氟化沉淀液为原料,采用单因素法对复杂MeSO4体系氟化沉淀除钙镁和复盐沉淀深度净化进行了研究. 氟化沉淀除钙镁实验结果表明,在温度90℃、时间1.0 h、pH 3.5及NH4F用量为理论量2.0倍的优化条件下,Ca2+和Mg2+的平均去除率分别为92.98%和89.95%. 复盐沉淀深度净化实验结果表明,硫酸铵的浓度和溶液酸度是复盐沉淀深度除Si的关键,优化条件为pH=1.5~2.5、游离硫酸铵浓度2.0~2.5 mol/L、时间1.0~1.5 h和室温. 在此条件下,Fe, Mn和Zn三种主体成分的沉淀率分别是69.94%, 86.52%和96.88%,Si的去除率为54.85%.
离子交换膜-硫酸铵溶液体系的极限电流密度
张晓燕;吕文华;丛威
. 2006, 6(6): 899-902.
摘要
(
)
PDF
(229KB) (
)
相关文章
|
计量指标
采用六室膜组合的膜堆研究离子交换膜-硫酸铵溶液体系的电流-电压曲线,考察了离子交换膜(JCM-15和JAM-15)-硫酸铵溶液体系中硫酸铵浓度、流速和温度对极限电流密度的影响. 实验结果表明,离子交换膜-硫酸铵溶液体系的电流-电压曲线明显有3个区域:欧姆区域、平缓增加区域和过极限电流区域. 增加硫酸铵浓度、流速和操作温度均能提高单极膜的极限电流密度. 在相同的操作条件下,阴膜(JAM-15)的极限电流密度明显高于阳膜(JCM-15). 离子交换膜-硫酸铵溶液体系的极限电流密度与流速和硫酸铵浓度的关系符合Wilson修正式,对本工作所采用的膜,ilim=17.647C0.4570V0.5725(JAM-15), ilim=13.003C0.2918V0.3697(JCM-15).
新型钾分子筛的表征及其对K+的交换性能
袁俊生;郭兆寿;张林栋
. 2006, 6(6): 903-906.
摘要
(
)
PDF
(306KB) (
)
相关文章
|
计量指标
通过扫描电镜、化学组成分析、X射线衍射和热重差热分析对自制的新型分子筛进行了表征,并测定了分子筛对纯钾溶液和海水中K+的交换容量及对K+的选择性系数. 结果表明,新型分子筛由76.25%的Na6Al6Si10O32×12H2O和23.75%的K2Al2Si3O10×3H2O两种物质混合构成,其硅铝比(摩尔比)为5.22;分子筛在350℃以内是稳定的,温度过高,内部结构被破坏;分子筛对纯钾溶液和海水钾离子的交换容量分别为100.30和55.10 mg/g,对海水中K+的选择性系数达到74.41,与改性天然沸石相比,对海水中K+的交换容量提高2倍,选择性系数提高3倍. 说明新型分子筛对K+具有很高的选择性,可用于从海水及含钾卤水中高选择性分离钾盐.
Synthesis, Characterization and Surface Properties of Cross-linked Polyurethane Dispersions Modified by Organosiloxane
高明志;许戈文
. 2006, 6(6): 907-911.
摘要
(
)
PDF
(147KB) (
)
相关文章
|
计量指标
A series of cross-linked polyether-polyester polyurethane dispersions modified with organosiloxane were prepared based on hydroxyl-terminated polydimethylsiloxane (HTPS) as hydrophobic component and 3-aminopropyl-triethoxysilane (APTS) as cross-linker as well as a bridge between polyurethane (PU) and polysiloxane (PSIL). It was discovered that polydimethylsiloxane segments were incorporated into PU chains chemically and organosiloxane was preferentially oriented toward the surface layer of the film by making a comparison of attenuated total reflection (ATR) spectra between the copolymer and the blend of PU and PSIL, which was further confirmed by investigation of electron spectroscopy for chemical analysis (ESCA). The relationships between surface properties of the film formed from polyurethane dispersion and organosiloxane content were also studied. The results showed that water contact angle of the film increased with the increase of organosiloxane content. Interestingly, it was also found that water contact angle of PUS film increased firstly and then decreased when film-forming temperature varied from 25℃ to 55℃.
过程与工艺
10-羟基喜树碱水溶性磷酰化衍生物的合成
杨柳;徐春艳;贾梦秋
. 2006, 6(6): 912-916.
摘要
(
)
PDF
(225KB) (
)
相关文章
|
计量指标
以10-羟基喜树碱(HCPT)为原料,吡啶为溶剂,经过磷酰化、酯化、水解三步反应合成了全新的水溶性磷酰化衍生物. 得到的较佳工艺条件为:磷酰化反应三氯氧磷与HCPT的投料摩尔比2:1(相对0.01 mol HCPT),反应温度-10℃,搅拌下反应时间30 min;酯化反应乙醇与HCPT的投料摩尔比6:1,反应温度10℃,搅拌下反应时间1.5 h;水解反应保持体系pH<5.0. ODS制备柱分离得到产物,总收率为30.0%.
硼铁矿碳热还原过程中的挥发
刘然;薛向欣;姜涛;段培宁;黄大威;王杏娟
. 2006, 6(6): 917-921.
摘要
(
)
PDF
(334KB) (
)
相关文章
|
计量指标
在热力学分析的基础上,研究了碳热还原硼铁矿过程中硼、镁的还原挥发行为. 实验表明,试样的总失重率随着温度的升高而增大,在1400~1450℃时很快达到最大值61.8%. B2O3始终存在着挥发失重,最大失重率达37.9%,MgO最大失重率达98.0%. 炉管口处的沉积物中B2O3含量为12.49%,证实了硼、镁的挥发现象.
TS-1分子筛催化苯乙酮氨肟化反应
章永洁;王亚权;刘腾飞;米镇涛;吴魏;闵恩泽;齐涛
. 2006, 6(6): 922-925.
摘要
(
)
PDF
(159KB) (
)
相关文章
|
计量指标
研究了钛硅分子筛(TS-1)催化苯乙酮氨肟化反应中溶剂、反应温度、助催化剂(氧化铝和乙酸铵)、氨水及H2O2用量对反应的影响. 结果表明,适宜的溶剂为乙醇,最佳反应温度为80℃,助催化剂乙酸铵在溶液中的浓度不低于0.43%(w)时能显著提高苯乙酮氨肟反应的转化率,而Al2O3的作用不明显. 为了获得较高的转化率,物料中NH3/苯乙酮以及H2O2/苯乙酮的摩尔比应分别控制在2.00和1.27以上.
系统与集成
乙烯淤浆聚合物体系的相平衡计算
沈航;顾雪萍;冯连芳;汤志武;刘波
. 2006, 6(6): 926-931.
摘要
(
)
PDF
(194KB) (
)
相关文章
|
计量指标
乙烯淤浆聚合反应体系的流程模拟与优化过程中气液相平衡的准确计算影响到聚乙烯生成量和聚乙烯分子量的模拟. 通过再参数化含链扰动统计缔合流体理论(Perturbed-Chain Statistical Associating Fluid Theory, PC-SAFT)状态方程,建立了乙烯淤浆聚合体系物性的计算方法. 以文献数据为基准,利用Polymers Plus软件平台,分别得到了乙烯、氢气、己烷、聚乙烯、氮气纯组分的PC-SAFT方程的模型参数,并在准确确定纯组分模型参数的基础上,得到了乙烯-己烷、氢气-己烷、氮气-己烷、以及聚乙烯-乙烯、聚乙烯-己烷组分二元交互系数. 计算结果表明,采用再参数化PC-SAFT状态方程可以准确计算乙烯淤浆聚合反应体系的纯组分物质性质和两组分之间的相平衡. 同时对工业过程中5个不同牌号聚乙烯的反应器内气液平衡状态进行了模拟计算,氢气与乙烯在气相的摩尔比与工业分析值能很好地吻合,最大误差为7.5%.
Combined Water-Oxygen Pinch Analysis with Mathematical Programming for Wastewater Treatment
宋丽丽;都健;柴绍斌;姚平经
. 2006, 6(6): 932-936.
摘要
(
)
PDF
(118KB) (
)
相关文章
|
计量指标
Water-oxygen pinch analysis is an effective method to decrease the wastewater quantity and improve the wastewater quality. But when multiple-contaminants are present, the method is difficult to be carried out. In this paper, the method that combines water-oxygen pinch analysis with mathematical programming is proposed. It obtains the general optimal solution and leads to the reuse stream that cannot be found only by pinch analysis. The new method is illustrated by an example, and the annual cost is reduced by 8.43% compared with the solution of literature.
组合式干燥系统的分段优化设计方法
王胜玮;胡仰栋;安维中;伍联营
. 2006, 6(6): 937-941.
摘要
(
)
PDF
(189KB) (
)
相关文章
|
计量指标
提出了分离过程的分段设计法:将一个任务分解为多个子任务,根据各个子任务的不同特点进行设计. 对干燥过程进行优化设计,以年费用最小为目标,将干燥过程表示为最多3段的超结构,每段有2个干燥设备可以选择,给出了单元和过程系统的模型和经济模型. 实例研究结果表明,当物料含水量大于物料在该条件下的临界含水量时,宜采用两段干燥的方法,将回转圆筒干燥器和流化床干燥器组合进行干燥;当物料含水量低于临界含水量时,宜采用一段干燥,将物料直接放入流化床干燥器进行干燥.
生化工程专栏
光温条件对新疆雪莲愈伤组织反应器培养后再分化能力的影响
雷亮;王晓东;徐春明;赵兵;王玉春
. 2006, 6(6): 942-947.
摘要
(
)
PDF
(247KB) (
)
相关文章
|
计量指标
研究了光质、光周期、昼夜温差和低温处理时间对反应器大规模培养后的新疆雪莲愈伤组织再分化能力的影响. 实验结果表明,长波长光更有利于愈伤组织的再分化. 光照时间显著影响愈伤组织的再分化能力,光照时间为16 h/d时愈伤组织的分化频率和平均出芽数达到最大,分别为76.7%和1.8个/块. 昼夜温差与愈伤组织的再分化能力呈显著负相关. 与水母雪莲不同,低温处理并不利于新疆雪莲愈伤组织的再分化. 新疆雪莲愈伤组织的再分化能力与同工酶的种类和活性密切相关.
重组大肠杆菌共表达D-海因酶和N-氨甲酰基-D-氨基酸酰胺水解酶
胡晓佳;李强;丛进阳
. 2006, 6(6): 948-953.
摘要
(
)
PDF
(356KB) (
)
相关文章
|
计量指标
通过PCR分别扩增得到N-carbamoylase基因和上游带有RBS区的D-hydantoinase基因,并将其依次克隆入pBAD/His A质粒中,得到呈多顺反子结构的双酶表达质粒pBAD-CRH,转化E. coli Top10F¢得到重组菌TaraCRH. 实验证明,E. coli TaraCRH对外源蛋白的表达控制严紧,而加入阿拉伯糖诱导后可以成功表达两酶基因. 诱导条件优化结果表明,诱导温度采用29℃,培养基中阿拉伯糖浓度0.05 g/L可达到最高酶活. 进一步尝试采用玉米浆培养基代替LB培养基,在经过优化的玉米浆培养基中培养TaraCRH菌株,经阿拉伯糖诱导,海因酶和水解酶酶活分别达到3.52和4.21 U/mL.
多孔聚(甲基丙烯酸环氧丙酯-二乙烯基苯)微球的改性及作为蛋白质疏水层析介质的应用
张颖;王仁伟;马光辉;谭天伟;苏志国
. 2006, 6(6): 954-958.
摘要
(
)
PDF
(289KB) (
)
相关文章
|
计量指标
用悬浮聚合方法合成了富含环氧基团的多孔聚(甲基丙烯酸环氧丙酯-二乙烯基苯) [Poly(Glycidyl Methacrylate-Divinylbenzene), P(GMA-DVB)]微球,为了消除其对蛋白质的不可逆吸附,探索用聚乙二醇(Polyethylene Glycol, PEG)对微球进行改性,制备了带有PEG配基的P(GMA-DVB)微球. 实验考察了反应条件对PEG固载量的影响规律,发现最适反应温度为80℃. 以牛血清白蛋白(Bovine Serum Albumin, BSA)和胰蛋白酶作为模型蛋白,考察了PEG改性前后P(GMA-DVB)微球对蛋白质的吸附性能. 改性前P(GMA-DVB)微球有30%~40%的不可逆吸附,蛋白质回收率仅为60%~70%. 改性后介质消除了不可逆吸附,对蛋白质的吸附作用表现为可逆的疏水相互作用,吸附BSA和胰蛋白酶的质量回收率和活性回收率都在97%以上. 结果表明,PEG-P(GMA-DVB)微球可以作为一种新型介质进一步应用于蛋白质的吸附与分离.
直接偶联法制备配基密度可控的丁基琼脂糖层析介质
冯清正;孟庆强;王佳兴;马光辉;马润宇;苏志国
. 2006, 6(6): 959-963.
摘要
(
)
PDF
(199KB) (
)
相关文章
|
计量指标
以快流速琼脂糖凝胶为基质,采用直接偶联法制备丁基琼脂糖疏水层析介质. 考察了影响反应的主要因素,通过四因素三水平正交实验和单因素实验,确定丁基琼脂糖疏水层析介质的优化反应条件为:反应温度45℃,反应时间45 min,催化剂三氟化硼乙醚用量0.02 mL/g. 在此条件下严格控制琼脂糖凝胶的含水量,改变丁基缩水甘油醚用量,制备了不同丁基密度的丁基琼脂糖疏水层析介质. 用不同密度的系列介质考察对牛血清白蛋白的吸附性能,初步研究了配基密度与吸附性能的关系;研究了疏水层析介质的机械稳定性和化学稳定性. 结果表明,其各项性能良好,具有广阔的应用前景.
复相乳化法制备海藻酸钙微球及其释放行为
张杰;郭妮妮;张代佳;修志龙
. 2006, 6(6): 964-968.
摘要
(
)
PDF
(309KB) (
)
相关文章
|
计量指标
采用复相乳化法制备了载牛血清白蛋白(BSA)的海藻酸钙微球,通过正交实验和单因素分析,以BSA包埋率、微球的载药率和平均粒径为考察指标,优化了该方法的制备参数,使最终制备的微球平均粒径小于10 mm,球形度较好,包埋率约70%,载药率达4%. 随着海藻酸钠质量分数的降低和BSA质量的增大,微球的包埋率下降、载药率升高、平均粒径减小. 微囊化BSA的体外释放曲线表明,该系统存在pH响应特性,尤其在磷酸缓冲液中,被包埋BSA的释放速率较快. 电泳结果表明,BSA的分子结构并未受制备过程的影响. 因此,该微囊化方法有望用于蛋白类药物的控释制剂,使其免受胃酸等的破坏,达到肠部释药的目的.
转光膜在雨生红球藻养殖上的应用
吴霞;康瑞娟;丛威;谭天伟
. 2006, 6(6): 969-972.
摘要
(
)
PDF
(288KB) (
)
相关文章
|
计量指标
通过对雨生红球藻在不同光质条件下生长的比较,确定了红色光有利于藻生长,进而用2.5 L气升式光照反应器在转光膜及普通PE膜下培养藻进行对比,结果显示雨生红球藻生物量、色素、光合活性等几项生物指标在转光膜条件下明显高于普通PE膜. 在气升式反应器内培养的藻细胞,接种9 d,虾青素含量可达3.57 mg/L,叶绿素浓度达到12.42 mg/L,干重提高8.8%以上.
材料工程专栏
轧制复合-粉末冶金发泡工艺制备泡沫铝夹心板
祖国胤;张敏;姚广春;李红斌
. 2006, 6(6): 973-977.
摘要
(
)
PDF
(463KB) (
)
相关文章
|
计量指标
针对目前泡沫铝夹心板制备工艺中存在的主要问题,将轧制复合技术应用于可发泡复合板的制备,以获得更高的芯层粉末致密度与界面结合强度. 研究结果表明,预压成型后的芯层粉体通过轧制过程能够同钢面板实现牢固的初结合,轧后芯层粉末的致密度明显高于热压复合板,粉末颗粒间呈紧密的层片状结构,为发泡过程创造了有利条件. 综合考虑界面结合强度、芯层粉末致密度及轧制缺陷等因素,轧制压下率应控制在60%~70%为宜. 复合板在适宜的发泡工艺下可以获得理想的泡沫体结构,最佳发泡温度为620~640℃,发泡时间为8~10 min. 发泡后在界面上生成了厚度均约为10 μm的金属间化合物FeAl3及Fe/Al固溶体,无脆性金属间化合物Fe2Al5生成,界面形成了理想的冶金结合.
泡沫铝材的泡体演化过程
郭志强;姚广春;尉海军;李红斌
. 2006, 6(6): 978-982.
摘要
(
)
PDF
(512KB) (
)
相关文章
|
计量指标
采用冷压和冷压+热压两种压制方式进行了对比实验,研究了压制方式对粉末冶金法制备泡沫铝材料的影响. 通过对在680℃保温发泡制备的泡沫铝的研究,得出了Al-Si-Ca合金粉末制备的泡沫铝材料的泡体演化过程. 泡体经历了形核、长大、坍塌3个过程,泡体形状也经历了从圆形到多边形的转变,最终在重力和毛细作用力的驱动下,气泡壁熔体流动引起气泡合并粗化,泡体底部出现实铝层,泡体开始坍塌.
锂离子电池负极Sn/Ni3Sn4合金的制备和表征
袁庆丰;卜冬蕾;王文璐;陈春华
. 2006, 6(6): 983-986.
摘要
(
)
PDF
(288KB) (
)
相关文章
|
计量指标
采用湿化学还原法及高能球磨处理工艺制备了Sn/Ni3Sn4双相合金体系,用XRD和SEM对其晶体结构和颗粒形貌进行了分析,以循环伏安法和恒电流循环对其电化学性能进行了表征. 结果表明,Sn/Ni3Sn4合金相由1~4 mm的团聚体组成. 该合金材料表现出96.4%的首次库仑效率和较高的比容量. 截止电压对其循环性能有很大的影响,0.3~1.0 V的电压区间显示出相对优良的循环稳定性.
Ca0.6Mg0.4Zr4(PO4)6耐碱腐蚀涂层制备及其性能
周健儿;许爱民;张小珍;王艳香;汪永清
. 2006, 6(6): 987-990.
摘要
(
)
PDF
(517KB) (
)
相关文章
|
计量指标
采用溶胶-凝胶法和浸渍涂覆技术在堇青石基体上成功制备了Ca0.6Mg0.4Zr4(PO4)6涂层. 采用XRD, SEM等分析测试手段对涂层的物相组成、表面和断面形貌进行了分析. 结果表明,制备的涂层为单相的Ca0.6Mg0.4Zr4(PO4)6,涂层致密无裂纹,主要由粒径2~3 mm的颗粒组成,涂层与基体间结合良好,涂层具有较好的高温耐碱腐蚀能力,涂覆该涂层可显著提高堇青石基体的高温耐碱腐蚀能力,3次涂覆试样在1000℃下经96 h碱蒸汽腐蚀后,涂层结构完好,试样的质量损失和强度下降率分别为0.9%和10.2%,远低于未涂覆涂层试样的质量损失8.2%和强度下降率87.2%.
综述
聚焦结构、界面与多尺度问题,开辟化学工程的新里程
李洪钟
. 2006, 6(6): 991-996.
摘要
(
)
PDF
(268KB) (
)
相关文章
|
计量指标
20世纪90年代以来,随着计算机技术和测量仪器的迅速发展,化学工程的研究水平日益提升,由经验规则的判断逐渐提高到计算机模拟量化分析. 化学工程的研究范围也日益扩大,下至纳微尺度结构与界面的观察与量化,上至宏观尺度设备与工厂的系统集成. 化学工程的服务对象也由化学工业扩展到冶金、材料、能源、环境、生物等诸多进行物质转化的过程工业. 目前化工科技界正在呼吁寻求继第一里程单元操作、第二里程传递过程和化学反应工程之后的第三里程. 化学工程中以往惯用的忽视非均匀多尺度结构和界面存在的平均方法是造成预测偏差和调控、放大困难的主要原因. 必须关注结构、界面和多尺度问题,研究多尺度结构、界面的量化预测理论和优化调控方法,建立多尺度结构、界面与"三传一反"的关系模型,与当代先进的计算方法、计算流体力学和计算机模拟相结合,有望解决化工过程与设备的优化调控与放大的难题,成为化学工程发展的新里程.
Progress of Gas Hydrate Studies in China
樊栓狮;汪集旸
. 2006, 6(6): 997-1003.
摘要
(
)
PDF
(356KB) (
)
相关文章
|
计量指标
A brief overview is given on the gas hydrate-related research activities carried out by Chinese researchers in the past 15 years. The content involves: (1) Historical review. Introducing the gas hydrate research history in China; (2) Gas hydrate research groups in China. There are nearly 20 groups engaged in gas hydrate research now; (3) Present studies. Including fundamental studies, status of the exploration of natural gas hydrate resources in the South China Sea region, and development of hydrate-based new techniques; (4) Future development.
循环流化床燃煤过程NOx和N2O产生-控制研究进展
张 磊;杨学民;谢建军;丁同利;姚建中;宋文立;林伟刚
. 2006, 6(6): 1004-1010.
摘要
(
)
PDF
(250KB) (
)
相关文章
|
计量指标
循环流化床(CFB)燃烧技术因其燃料适应范围广、污染物排放低等优点,近几十年得到广泛应用. 随着当前环保要求的日益提高,CFB燃煤过程N2O排放浓度较高成为其应用的瓶颈问题. 因此系统总结CFB燃煤过程中NOx和N2O排放的研究现状对开发新型CFB燃煤技术具有重要意义. 本工作首先讨论了CFB燃煤过程中NOx和N2O的均相和异相反应机理,然后应用这些机理分析了床温、过剩空气系数、分级燃烧,以及煤种对CFB燃煤过程NOx和N2O排放的影响. 在此基础上,对常见的抑制NOx和N2O排放的工艺从机理角度进行了归纳总结. 最后,对2种本工作认为有应用前景的CFB燃煤减排NOx和N2O新技术?反向分级燃烧技术及CFB解耦燃烧技术进行了简要论述.
甲酸脱氢酶用于辅酶NADH再生的研究进展
黄志华;刘铭;王宝光;张延平;曹竹安
. 2006, 6(6): 1011-1016.
摘要
(
)
PDF
(204KB) (
)
相关文章
|
计量指标
NADH依赖型氧化还原酶广泛应用于精细化学品和手性化合物的生物合成,其中辅酶NADH作为还原当量起着关键的作用,NADH的再生关系到生物氧化还原过程能否进行. 甲酸脱氢酶在辅酶NADH再生中的应用是目前代谢工程领域研究的热点之一. 本工作回顾了甲酸脱氢酶的来源和氨基酸序列、酶的理化性质和催化机理等方面的研究进展,从化学稳定性、热稳定性和成本等方面阐述了甲酸脱氢酶在辅酶再生系统中的应用,讨论了甲酸脱氢酶用于辅酶再生的代谢工程平台的发展趋势,并对研究发展方向提出了一些设想.